Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.30 MPa | 479 psi | ASTM D412 |
Polymax® Maxelast® P1840P TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 3.30 MPa | 479 psi | ASTM D412 |
Polymax® Maxelast® P2855B TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 3.30 MPa | 479 psi | ASTM D638 |
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® KU 2-8671 Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
|
Daikin DAI-EL G-763 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability for O-rings.Information provided by Daiki.. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
|
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Tensile Strength, Yield | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc.. |
|||
Tensile Strength, Yield | 3.30 MPa | 479 psi | M100 |
3M Dyneon™ Aflas® FA-100S PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |