Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.31 MPa | 480 psi | 200%, post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7727 TLC Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7727 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7265D Fluorocarbon-Elastomer Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3201-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3210-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3301-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3310-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 3.31 MPa @Strain 300 % |
480 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 38-096 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerOpaqueApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDisclai.. |
|||
Tensile Strength, Yield | 3.31 MPa @Strain 300 % |
480 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 702 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection MoldingPolyOne.. |
|||
Tensile Strength, Yield | 3.31 MPa | 480 psi | at 100%; ASTM D412 |
G-2701 Styrene-based Biomedical Elastomer |