Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 480 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.31 MPa
480 psi
200%, post cured- 4 hours at 204°C
Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.31 MPa
480 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.31 MPa
480 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.31 MPa
480 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7727 TLC Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tensile Strength, Yield 3.31 MPa
480 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7727 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tensile Strength, Yield 3.31 MPa
480 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7265D Fluorocarbon-Elastomer
Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 3.31 MPa
480 psi
100%; ASTM D412
Teknor Apex APEX® 3201-55 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 3.31 MPa
480 psi
100%; ASTM D412
Teknor Apex APEX® 3210-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 3.31 MPa
480 psi
100%; ASTM D412
Teknor Apex APEX® 3301-55 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 3.31 MPa
480 psi
100%; ASTM D412
Teknor Apex APEX® 3310-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Tensile Strength, Yield 3.31 MPa

@Strain 300 %
480 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 38-096 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerOpaqueApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDisclai..
Tensile Strength, Yield 3.31 MPa

@Strain 300 %
480 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 702 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection MoldingPolyOne..
Tensile Strength, Yield 3.31 MPa
480 psi
at 100%; ASTM D412
G-2701 Styrene-based Biomedical Elastomer
Copyright © lookpolymers.com All Rights Reserved