Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.62 MPa
525 psi
ASTM D412
Polymax® Maxelast® C4650 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Strength, Yield 3.62 MPa
525 psi
ASTM D412
Polymax® Maxelast® P1755 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 3.62 MPa
525 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5724 Fluorocarbon-Elastomer
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 3.62 MPa
525 psi
ASTM D412
Teknor Apex UNIPRENE® 7100-45 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 3.62 MPa
525 psi
ASTM D412
Teknor Apex Uniprene® UN-1141A Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..