Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3040 psi
Spartech E65390 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
Tensile Strength, Yield 21.0 MPa
3040 psi
ASTM D412
Teknor Apex APEX® 1700-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met..
Tensile Strength, Yield 21.0 MPa
3040 psi
2.0 in/min; ASTM D638
ExxonMobil PP143KNE1 Polypropylene Homopolymer
Product Description: A high impact copolymer resin designed consumer and industrial applications.Availability: North America Features:Good ColorabilityGood Dimensional StabilityGood Mold ReleaseGoo..
Tensile Strength, Yield 21.0 MPa
3040 psi
2.0 in/min; ASTM D638
ExxonMobil PP7505KNE2 Polypropylene Homopolymer
Product Description: A medium to high impact copolymer designed for injection molded large consumer and industrial parts requiring high melt flow rate.Availability: North America Features:Balanced ..
Tensile Strength, Yield 21.0 MPa
3040 psi
2.0 in/min; ASTM D638
ExxonMobil PP8255E1 Polypropylene Homopolymer
Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes...