Material Notes:
Product Description: A high impact copolymer resin designed consumer and industrial applications.Availability: North America Features:Good ColorabilityGood Dimensional StabilityGood Mold ReleaseGood Thermal StabilityMedium FlowNucleatedUses: ContainersIndustrial ApplicationsPalletsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3040 psi
2.0 in/min; ASTM D638
Elongation at Yield 5.1 %
5.1 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1100 MPa
159000 psi
0.5 in/min; ASTM D790A
Izod Impact, Notched NB
NB
ASTM D256A
Gardner Impact 33.8 J

@Thickness 3.17 mm,
Temperature -28.9 °C
24.9 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C
196 °F
ASTM D648
Users viewing this material also viewed the following: