Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.06 MPa
5085 psi
ASTM D412
Lubrizol Advanced Materials PEARLCOAT® Activa D126K BL Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLCOAT® Activa D126K BL is a standard polyester based TPU, supplied in form of translucent, black colored pellets, combining hardness with excellent low-temperature flexibility. PEARLCOAT® Acti..
Tensile Strength, Yield 35.06 MPa
5085 psi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec..