Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 36.7 MPa | 5320 psi | 88% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 36.7 MPa | 5330 psi | ASTM D-638 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 36.7 MPa | 5330 psi | ASTM D-638 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 36.7 MPa | 5320 psi | |
Ineos ABS Centrex® 825 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi.. |