Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 248 MPa | 36000 psi | |
PSM Industries Pacific Sintered Metals Bronze BT-126 Powdered Metal Higher strength structural and bearing bronzeInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 248 MPa @Strain 0.200 %, Temperature 649 °C |
36000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 248 MPa @Strain 0.200 %, Temperature 538 °C |
36000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 248 MPa @Strain 0.200 %, Temperature 204 °C |
36000 psi @Strain 0.200 %, Temperature 399 °F |
|
Haynes Hastelloy® G-30® alloy, plate and bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 248 MPa | 36000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF55 HS L 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Tensile Strength, Yield | 248 MPa | 36000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF55 HS L OR016 57% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 57% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Tensile Strength, Yield | 248 MPa | 36000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF60 TL10 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 8575101Information provi.. |
|||
Tensile Strength, Yield | 248 MPa | 36000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant, UV Stabilized and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessing Method: Inject.. |
|||
Tensile Strength, Yield | 248 - 421 MPa | 36000 - 61000 psi | 0.2% offset |
Eagle Brass 194 HSM® Copper, 1/2 Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Yield | 248 MPa | 36000 psi | |
Pacific Sintered Materials BT-126 Bronze Powdered Metal Applications: Higher strength structural and bearing bronze.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 248 MPa @Strain 0.200 %, Temperature 316 °C |
36000 psi @Strain 0.200 %, Temperature 601 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |