Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.50 - 28.3 MPa
363 - 4110 psi
Average value: 7.13 MPa Grade Count:24
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Tensile Strength, Yield >= 2.50 MPa
>= 363 psi
Trelleborg Offshore Vikotherm™ 73961 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Tensile Strength, Yield >= 2.50 MPa
>= 363 psi
Trelleborg Offshore Vikotherm™ 73982 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Tensile Strength, Yield 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 527-1/-2
Covestro Desmopan® DP 1960AW Polyurethane
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Tensile Strength, Yield 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 527-1/-2
Covestro Desmopan® DP 1966AW Polyurethane
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Tensile Strength, Yield 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 527-1/-2
Covestro Desmopan® DP 3070AU Polyurethane
injection molding gradefree from plasticizersApplicationInjection molded engineering partshard - soft systemsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially ..
Tensile Strength, Yield 2.50 MPa
363 psi
Dow AFFINITY™ SM 8250 Polyolefin Plastomer
AFFINITY® SM 8250 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in injection molded clear or colored flexible durable parts. It exhibits excellent clarity and flex..
Tensile Strength, Yield 2.50 MPa
363 psi
508 mm/min; ASTM D638
Dow Engage® 8452 Polyolefin Elastomer
Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin..
Tensile Strength, Yield 2.50 MPa
363 psi
ACC MM282 Specialist Molding 2-Part Condensation Cure
Part of the Amber Chemical Group. Data provided by manufacturer.
Tensile Strength, Yield 2.50 MPa
363 psi
ACC MM911 Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing..
Tensile Strength, Yield 2.50 MPa
363 psi
50 mm/min
Arkema Group Evatane® 1350 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets.ISO data provided by the manufacturer, Arkema.