Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.48 - 26.2 MPa | 1230 - 3800 psi | Average value: 13.0 MPa Grade Count:22 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Tensile Strength, Yield | 17.6 - 26.2 MPa | 2550 - 3800 psi | Average value: 21.3 MPa Grade Count:9 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |