Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.48 MPa | 1230 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR MF5420-0085 NHFR Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | ASTM D412 |
Polymax® Maxelast® D6975CT TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | ASTM D412 |
Polymax® Maxelast® P1790 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | ASTM D412 |
Polymax® Maxelast® P3785H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | ASTM D412 |
Polymax® Maxelast® P3865A TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | ASTM D412 |
Polymax® Maxelast® P3870 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | >= 8.50 MPa | >= 1230 psi | -15% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering C70H Chloroprene Rubber Off-white, Chloroprene Rubber, 65-75 °IRHD. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regu.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | -15% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering E65K Ethylene Propylene Rubber Peroxide cured, Ethylene Propylene Terpolymer (EPT), 50-70 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing sulphur hexafluoride (SF6) gas in electric.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | ASTM D412 |
Precision Polymer Engineering N50M Nitrile Rubber Nitrile Butadiene Rubber, 48-58 °IRHD. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Standard BS2751 BA50.Applications: Excellent resistance to petro.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | -15% change after 70 hours @ 70°C; ASTM D412 |
Precision Polymer Engineering N60M Nitrile Rubber Nitrile Butadiene Rubber (NBR) 55-65 °IRHD. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet specification BS2751 BA60. Also meets obsolescent specification BS3.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | ASTM D412 |
Precision Polymer Engineering S80U Silicone Rubber Translucent Silicone Rubber, 70 -80 °IRHD. Shore A Platinum cured Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Silicone compound in conformity with the req.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | ASTM D638 |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7145 Fluorocarbon-Elastomer FKM specially for oil & gas service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | |
Spartech E65450 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | |
Spartech M60450 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | ASTM D412 |
Teknor Apex Flexalloy® 3500-45 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 8.47 MPa @Treatment Temp. 200 °C, Time 252000 sec |
1230 psi @Treatment Temp. 392 °F, Time 70.0 hour |
Heat Aging; ASTM D573 |
Vicone High Performance Rubber VicoFluor™ C105LF-BL High Performance Fluoroelastomer Information provided by Vicone |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | |
Trelleborg B429 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | |
Trelleborg R439 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | |
Trelleborg Z500 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Tensile Strength, Yield | 8.50 MPa @Strain 100 % |
1230 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1490A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldinghigh melt stabilityvery large processing windowApplicationBellowsInjection molded engineering partsO-stringsHosesnon-reinforc.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | |
Dow Primacor® 2912 Ethylene Acrylic Acid (EAA) PRIMACOR® 2912 polymer containing 9.5% comonomer is an extrusion/ coextrusion coating resin for flexible packaging applications. It is designed to provide excellent adhesion to metallic, paper and .. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | |
Dow Primacor® 3330 Ethylene Acrylic Acid (EAA) PRIMACOR® 3330 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent toughness, environmenta.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | 50 mm/min |
Arkema Group Evatane® 1020 VB 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for transparent, resistant films, sealable at low temperature. Examples: laminates.ISO data provided by the manufacturer, Arke.. |
|||
Tensile Strength, Yield | 8.50 MPa | 1230 psi | 50 mm/min |
Arkema Group Evatane® 1020 VG 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for resistant films, sealable at low temperature with some hot tack. Examples: bags, deep-freeze packaging, laminates, coextru.. |
|||
Tensile Strength, Yield | 8.50 MPa @Strain 100 % |
1230 psi @Strain 100 % |
|
Daikin DAI-EL G-912 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good compression set.Information provided by Daikin Industries. |
|||
Tensile Strength, Yield | 8.48 - 26.2 MPa | 1230 - 3800 psi | Average value: 13.0 MPa Grade Count:22 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3780 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |
|||
Tensile Strength, Yield | 8.48 MPa | 1230 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene LDPE 023919 features good heat sealing latitude and easy processability. Applications include food contact, squeeze bottles, and non-escr.Former A-Top Polymers product; part of Amco product line sin.. |