Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 262 MPa @Temperature 23.9 °C |
38000 psi @Temperature 75.0 °F |
Dry; ASTM D638 |
Park Electrochemical Nelcote® P-601 Polyester Prepreg, 18oz. Woven Fiberglass Roving P-601 Polyester is a fire retardant prepreg resin system, which meets the requirements of MIL-R-7575. P-601 prepregs are available on any style of woven fiberglass fabric having a suitable finish, s.. |
|||
Tensile Strength, Yield | 262 MPa | 38000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NN-40CF/000 - OBSOLETE Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 % |
38000 psi @Strain 0.200 % |
|
FloMet 316L Stainless Steel FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 %, Temperature 538 °C |
38000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 %, Temperature 204 °C |
38000 psi @Strain 0.200 %, Temperature 399 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 262 MPa @Temperature 871 °C |
38000 psi @Temperature 1600 °F |
|
Universal Wire Works 617 Nickel Alloy Welding Wire Alloy 617 is used for TIG and MIG welding of Inconel type alloy 617 and alloys of similar composition. Alloy 617 welds produce high stress-rupture strength in prolonged exposure to high temperatures.. |
|||
Tensile Strength, Yield | >= 262 MPa | >= 38000 psi | Larger sizes may be lower. |
Alcoa Toolrite 2011®-T3 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Tensile Strength, Yield | 262 MPa | 38000 psi | |
CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 % |
38000 psi @Strain 0.200 % |
Annealed |
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 %, Temperature 204 °C |
38000 psi @Strain 0.200 %, Temperature 399 °F |
|
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 %, Temperature 149 °C |
38000 psi @Strain 0.200 %, Temperature 300 °F |
|
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 % |
38000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 800 & 800-H UNS N08800 & UNS N08810 Nickel Superalloy Corrosion-resistant alloy for petrochemical and food processing equipment, tubing, heat exchangers, and furnaces.Property values are for samples in the metallurgical condition: 2100°F anneal + wate.. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 %, Temperature 204 °C |
38000 psi @Strain 0.200 %, Temperature 399 °F |
|
AK Steel 309 Austenitic Stainless steel AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh.. |
|||
Tensile Strength, Yield | 262 MPa | 38000 psi | Offset not specified |
Carpenter HyMu "80"® Electronic Alloy, Strip, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |