Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.30 MPa | 624 psi | M100 |
3M Dyneon™ Fluorel™ FC-2261Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Tensile Strength, Yield | 4.30 MPa | 624 psi | At 100% elongation, across flow; ASTM D412 |
Advanced Elastomer Systems VistaFlex® 911-N Thermoplastic Rubber
(discontinued **) Description: A colorable high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as fr.. |
|||
Tensile Strength, Yield | 4.30 MPa @Strain 300 % |
624 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 9370A Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi.. |
|||
Tensile Strength, Yield | 4.30 MPa @Strain 300 % |
624 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 9370AU Polyurethane Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission r.. |
|||
Tensile Strength, Yield | 4.30 MPa | 624 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Softflex® SF 0450 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 4.30 MPa | 624 psi | Film Property, 50 µm thickness; ASTM D882 |
Arkema Group OREVAC® 9318 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Tensile Strength, Yield | 4.30 MPa @Strain 100 % |
624 psi @Strain 100 % |
ASTM D638 |
Toyobo E3080A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information .. |