Covestro Desmopan® DP 9370AU Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 9370AU Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable filmsFilmsSports shoe soleshard - soft systemsPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
3s; ISO 868
Tensile Strength at Break 25.0 MPa
3630 psi
ISO 527-1/-2
Tensile Strength, Yield 25.0 MPa
3630 psi
parallel; ISO 527-3
2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 527-1/-2
4.30 MPa

@Strain 300 %
624 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 69
69
mm³; ISO 4649
Compression Set 22 %

@Temperature 23.0 °C
22 %

@Temperature 73.4 °F
ISO 815
49 %

@Temperature 70.0 °C
49 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved