Polymer Property : Tensile Strength, Yield = 4.55054 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.55054 - 8.99766 MPa

@Temperature -55.0 - 177 °C
660.001 - 1305.00 psi

@Temperature -67.0 - 350 °F
Average value: 6.30 MPa Grade Count:7
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..