Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.55054 - 8.99766 MPa @Temperature -55.0 - 177 °C |
660.001 - 1305.00 psi @Temperature -67.0 - 350 °F |
Average value: 6.30 MPa Grade Count:7 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |