Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.57 MPa
663 psi
ASTM D412
Polymax® Maxelast® N8955 TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Tensile Strength, Yield 4.57 MPa
663 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5803 Fluoro-silicone
Fluoro-siliconeInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield >= 4.57 MPa
>= 663 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5404 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.