Seals Eastern 5404 Nitrile Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Seals Eastern, Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern 5404 Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose NitrileInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 80
>= 80
ASTM D2240, Type A
90
90
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 12.59 MPa
>= 1826 psi
ASTM D412 Method A
19.09 MPa
2769 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield >= 2.68 MPa
>= 389 psi
Stress at Elongation M50; ASTM D412 Method A
2.70 MPa
391 psi
AVG Stress at Elongation M25; ASTM D412 Method A
>= 4.57 MPa
>= 663 psi
Stress at Elongation M100; ASTM D412 Method A
4.59 MPa
666 psi
AVG Stress at Elongation M50; ASTM D412 Method A
10.34 MPa
1499 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 129 %
>= 129 %
ASTM D412 Method A
182 %
182 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.02031 GPa
2.946 ksi
ASTM D412 Method A
Shear Modulus 0.00677 GPa
0.982 ksi
ASTM D412 Method A
Secant Modulus 0.01909 GPa
2.769 ksi
ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 42