Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.76 MPa | 400 psi | at 200%, as molded |
Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | TM R050-36 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Tensile Strength, Yield | >= 2.76 MPa | >= 400 psi | No units listed, assumed to be psi. |
712BNF Cork/Nitrile Rubber Sheet Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot.. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 615 Perfluoroelastomer Greene Tweed’s Chemraz® 615 exhibits outstanding high temperature properties, with a temperature range from 0°F to 615°F (-18°C to 324°C). Chemraz 615’s chemical resistance.. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | at 100%; ASTM D412 |
Multibase Multi-Flex® A 7204 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F.. |
|||
Tensile Strength, Yield | >= 2.76 MPa | >= 400 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7145 Fluorocarbon-Elastomer FKM specially for oil & gas service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3201-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3310-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1037FL Thermoplastic Elastomer Notes: Transparent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1643L1 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1851 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1627L3 Thermoplastic Elastomer Features: Excellent Elastic Recovery; Tough; Good Melt Strength Uses: Strap ProductsInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1881 Thermoplastic Elastomer Uses: Grips Features: Excellent Resistance to Skin OilsInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 2770UV Thermoplastic Elastomer Notes: General Purpose; OpaqueInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 2860E Thermoplastic Elastomer Notes: Translucent Features: Good Chemical and Oil Resistance; Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1304 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1504 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt Strength Uses: Safety ProductsInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa @Strain 300 % |
400 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1564 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | Adhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412 |
Teknor Apex UNIPRENE® 7400-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | |
Master Bond Mastersil 410 One Component Room Temperature Curing Silicon Master Bond MasterSil 410 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This compound has a pas.. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | |
Master Bond Mastersil 711 Fast Curing One Component Silicone MasterSil 711 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This specialty product features an exceptional.. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | cured 72 hrs @ RT |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 086LFR Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Flame RetardantMulti-Purpose Thermoplastic ElastomerApplications:General PurposeInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Co.. |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | at 100%; ASTM D412 |
D-2103 Styrene-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | at 100%; ASTM D412 |
G-2705 Styrene-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 2.76 MPa | 400 psi | at 100%; ASTM D412 |
EG80A Polyurethane-based Biomedical Elastomer |