Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EG80A Polyurethane-based Biomedical Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EG80A Polyurethane-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
ASTM D2240
Tensile Strength, Ultimate 38.9 MPa
5640 psi
ASTM D412
Tensile Strength, Yield 2.76 MPa
400 psi
at 100%; ASTM D412
Elongation at Break 709 %
709 %
ASTM D412
Users viewing this material also viewed the following: