Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 28.8 MPa | 4170 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 28.8 MPa | 4170 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 28.8 MPa | 4170 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 28.8 MPa | 4170 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 28.8 MPa | 4170 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 28.8 MPa | 4170 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |