Polymer Property : Tensile Strength, Yield = 42.07 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.07 MPa
6102 psi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 11H94 Thermoplastic Polyurethane Elastomer
PEARLTHANE® D11H94 is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring adequate hardness as well as excellent flow and mech..
Tensile Strength, Yield 42.07 MPa
6102 psi
ASTM D638
Lucent Polymers ABS-305 Acrylonitrile Butadiene Styrene, General Purpose
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 42.07 MPa
6102 psi
ASTM D638
Lucent Polymers ABS-305LG Acrylonitrile Butadiene Styrene, General Purpose, Low Gloss
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.