Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers ABS-305LG Acrylonitrile Butadiene Styrene, General Purpose, Low Gloss

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers ABS-305LG Acrylonitrile Butadiene Styrene, General Purpose, Low Gloss.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
1/8" Section
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.07 MPa
6102 psi
ASTM D638
Elongation at Yield >= 10 %
>= 10 %
ASTM D638
Flexural Strength 74.48 MPa
10800 psi
ASTM D790
Flexural Modulus 2.2069 GPa
320.08 ksi
ASTM D790
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.001 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.78 °C
190.0 °F
ASTM D648
Users viewing this material also viewed the following: