Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 290 MPa @Temperature 100 °C |
42100 psi @Temperature 212 °F |
|
RSP Technology RSA-4019 AE Aluminum Super Alloy Precision Equipment, High Strength - High TempRSP Technology develops, produces and sells aluminium super alloys with high end properties. By using its own Meltspinning process, ultra fast cooling .. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 %, Temperature 649 °C |
42100 psi @Strain 0.200 %, Temperature 1200 °F |
|
Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched Typical applications include, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc. |
|||
Tensile Strength, Yield | >= 290 MPa | >= 42100 psi | |
MetalTek Nitronic® 50 Cast UNS J93790 Austenitic Stainless Steel Corrosion resistance and high strength. Produced under license of ARMCO Advanced Materials Corp. Applications: Deck equipment, pumps, valves.Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 290 MPa | >= 42100 psi | |
MetalTek Nitronic® 60 Cast UNS J92972 Austenitic Stainless Steel Wear and galling resistance. Produced under license of ARMCO Advanced Materials Corp. Applications: Pump wear rings, valve trim.Information provided by MetalTek |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 %, Temperature 540 °C |
42100 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 %, Temperature 760 °C |
42100 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes 556® alloy, all-weld metal GTAW Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 %, Temperature 425 °C |
42100 psi @Strain 0.200 %, Temperature 797 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 %, Temperature 650 °C |
42100 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 %, Temperature 316 °C |
42100 psi @Strain 0.200 %, Temperature 601 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 %, Temperature 93.0 °C |
42100 psi @Strain 0.200 %, Temperature 199 °F |
|
Haynes Hastelloy® G-30® alloy, plate and bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 290 MPa @Temperature 650 °C |
42100 psi @Temperature 1200 °F |
Annealed prior to test |
Special Metals INCONEL® Alloy 625 Niobium content includes tantalum. A nickel-chromium-molybdenum alloy with an addition of niobium that acts with the molybdenum to stiffen the alloy's matrix and thereby provide high strength witho.. |
|||
Tensile Strength, Yield | 290 MPa | 42100 psi | ASTM-D638 |
Polyram PlusTek PA303G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 290 - 380 MPa @Strain 0.200 % |
42100 - 55100 psi @Strain 0.200 % |
|
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 % |
42100 psi @Strain 0.200 % |
|
AK Steel 304 Austenitic Stainless steel AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. .. |
|||
Tensile Strength, Yield | 290 MPa | 42100 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 % |
42100 psi @Strain 0.200 % |
290 MPa is typical, Minimum per ASTM A240 is 205 MPa. |
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008) Allegheny Ludlum Al 410S™ stainless steel is a low-carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and /or columbium minimize austenite form.. |
|||
Tensile Strength, Yield | 290 MPa | 42100 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 0% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 % |
42100 psi @Strain 0.200 % |
|
AK Steel 316 Austenitic Stainless steel AK Steel 316 contains molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated tempe.. |
|||
Tensile Strength, Yield | 290 MPa | 42100 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 0% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 290 MPa | 42100 psi | |
Ametek 17-4 P/M Process, Sintered at 2050°F (1121°C) Composition reported is typical of 17-4 precipitation hardening stainless. This alloy is widely used because of its high strength, high hardness, excellent corrosion resistance, and easy heat treat.. |
|||
Tensile Strength, Yield | 290 MPa | 42100 psi | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Tensile Strength, Yield | 290 MPa @Strain 0.200 % |
42100 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC Allegheny Ludlum Type 410HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |