Mechanical Properties Metric English Comments
Tensile Strength, Yield 200 - 380 MPa
29000 - 55100 psi
Materion Beryllium Copper Alloy 25 Strip; A -Planished (TB00) Temper (UNS C17200)
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply ..
Tensile Strength, Yield 170 - 380 MPa
24700 - 55100 psi
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Tensile Strength, Yield 170 - 380 MPa
24700 - 55100 psi
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Tensile Strength, Yield 220 - 380 MPa
31900 - 55100 psi
Sinotek Materials CFC Carbon Heat Insulation Material
Information provided by Sinotek
Tensile Strength, Yield 290 - 380 MPa

@Strain 0.200 %
42100 - 55100 psi

@Strain 0.200 %
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Tensile Strength, Yield 300 - 380 MPa
43500 - 55100 psi
ArcelorMittal Dual Phase 500 Very high strength steel, Cold Rolled Steel
Available in the following: HCT600X (uncoated), HCT600X+ZE (electrogalvanized) and HCT600X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a..
Tensile Strength, Yield 340 - 380 MPa
49300 - 55100 psi
L direction
ArcelorMittal Torque 20-15 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Yield 340 - 380 MPa
49300 - 55100 psi
L direction
ArcelorMittal Torque 25-16 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Yield 340 - 380 MPa
49300 - 55100 psi
L direction
ArcelorMittal Torque 27-16 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Yield 340 - 380 MPa
49300 - 55100 psi
L direction
ArcelorMittal Torque 30-17 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Yield 340 - 380 MPa
49300 - 55100 psi
L direction
ArcelorMittal Torque 30-18 Electrical Steel
Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc..
Tensile Strength, Yield 300 - 380 MPa
43500 - 55100 psi
ArcelorMittal FB 450 Hot rolled ferrite-bainite steel
Available in the following: uncoated (HDT450F) and Extragal® (HDT450F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It compr..
Tensile Strength, Yield 300 - 380 MPa
43500 - 55100 psi
ArcelorMittal FF 280 D Very high strength steel, Cold Rolled Steel
Available in the following: HCT450X (uncoated), HCT450X+ZE (electrogalvanized) and HCT450X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a..