Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.2 MPa
6270 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L7005 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon L7005 is recommended for whites and light pastel colors only.Note: Physical properties based on L7005 tan 3210 sample.Information provided by PolyOne
Tensile Strength, Yield 43.2 MPa
6270 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L7007 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon L7007 is recommended for whites and light pastel colors only.Geon L7007 is a higher gloss version of L7005.Information provided by PolyOne
Tensile Strength, Yield 43.2 MPa

@Thickness 3.20 mm
6270 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG ..
Tensile Strength, Yield 43.2 MPa
6260 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SBB 3616 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P..
Tensile Strength, Yield 43.2 MPa
6270 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 3500
Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 43.2 MPa
6270 psi
ASTM D412
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Tensile Strength, Yield 43.2 MPa
6260 psi
ASTM D-638
Axiall 3101 Rigid PVC, Extrusion
Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be..
Tensile Strength, Yield 43.2 MPa
6260 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SBF 3758 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex