Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical LG709W ABS, Low Gloss, Heat Resistance Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG.. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® MG-0330 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0315 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR Flame-retardant ABS with high heat resistance that can be used in battery cases and adaptorsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR Flame-retardant ABS with high heat resistance that can be used in battery cases and adaptorsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.2 MPa | 6260 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBB 3616 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P.. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D638 |
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade Medium Impact, High Gloss, High FlowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D638 |
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.2 MPa | 6260 psi | ASTM D-638 |
Axiall 3101 Rigid PVC, Extrusion Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be.. |
|||
Tensile Strength, Yield | 43.2 MPa | 6260 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBF 3758 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |