Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.3 MPa | 6280 psi | 103% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 43.3 MPa | 6280 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 4001HH Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 43.3 MPa | 6280 psi | ASTM D412 |
C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |