Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer C.O.I.M. S.p.A.
Trade Name Laripur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGreat flexibility with constancy at temperature variationsGood compression resistanceGood water and light resistanceGood resistance to oils, fats and to many types of solventsSeries 60 and E 2103 PTMG Ether: These products are based on PTMG polyether. In comparison to the LARIPUR® ester series, they show a higher resistance to hydrolysis and microbiological attacks, have higher cold flexibility but have lower thermal and oxidizing resistance. Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ASTM D2240
Tensile Strength, Yield 43.3 MPa
6280 psi
ASTM D412
Elongation at Break 580 %
580 %
ASTM D412
50% Modulus 0.00500 GPa
0.725 ksi
ASTM D412
100% Modulus 0.00680 GPa
0.986 ksi
ASTM D412
300% Modulus 0.0155 GPa
2.25 ksi
ASTM D412
Tear Strength 70.0 kN/m
399 pli
ASTM D624
Abrasion 40
40
mm3, Abrasion Loss; DIN 53516
Compression Set 24 %
24 %
70 hours at 23°C; ASTM D395
42 %

@Temperature 70.0 °C
42 %

@Temperature 158 °F
Method B, 22 hours; ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Flammability, UL94 V-0
V-0
Vertical Burning
Descriptive Properties Value Comments
Features Flame Retardant, Transparent, Halogen Free
Users viewing this material also viewed the following: