Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 179 - 441 MPa | 26000 - 64000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, 1/4 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Yield | 103 - 441 MPa | 15000 - 64000 psi | |
Chicago Extruded Metals BioBrass® UNS C26000 Copper-Zinc Alloy Finished product available as bar, wire, rod or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext.. |