Material Notes:
Finished product available as bar, wire, rod or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.53 g/cc
0.308 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 60 - 82
60 - 82
Tensile Strength 324 - 896 MPa
47000 - 130000 psi
Tensile Strength, Yield 103 - 441 MPa
15000 - 64000 psi
Elongation at Break 3.0 - 66 %
3.0 - 66 %
Machinability 30 %
30 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 68.5 - 71.5 %
68.5 - 71.5 %
Iron, Fe 0.050 %
0.050 %
Lead, Pb 0.070 %
0.070 %
Other, total 0.30 %
0.30 %
Zinc, Zn 28.08 - 31.08 %
28.08 - 31.08 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000616 ohm-cm
0.00000616 ohm-cm