Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 47.1 - 120 MPa | 6830 - 17400 psi | Average value: 94.9 MPa Grade Count:48 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 50 mm/min; ASTM D638 |
LG Chemical 15NFE GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | ASTM D638 |
I. Stern GPPS-004 General Purpose Crystal Polystyrene Features:High Strength GradeMedium Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & C.. |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LI921NS ASA Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® TE5011M PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical XR490 ABS, Heat Resistance, Low Emission Feature: Injection Molding, Heat Resistance, Low EmissionApplication: Automotives Interior Housing (Glove Box Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG C.. |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® TE5011 PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® BC-0140 H ABS, Unreinforced General Purpose Stiff ABS material for automobile bobbinInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBB 3704 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Good Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provide.. |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBC 3710 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SRF 3703 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | ASTM D638 |
Cheng Yu Plastic PP236G1 Polypropylene, 10% Glass Fiber |
|||
Tensile Strength, Yield | 47.1 - 53.6 MPa | 6830 - 7770 psi | ASTM D638M |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-14S ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
Type 1; ASTM D638 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Tensile Strength, Yield | 47.1 MPa | 6830 psi | ASTM D638M |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-14S ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Tensile Strength, Yield | 47.1 MPa @Thickness 3.20 mm |
6830 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |