Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 - 120 MPa
3190 - 17400 psi
Average value: 57.4 MPa Grade Count:244
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Yield 47.1 - 120 MPa
6830 - 17400 psi
Average value: 94.9 MPa Grade Count:48
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Tensile Strength, Yield 45.0 - 120 MPa
6530 - 17400 psi
Average value: 82.5 MPa Grade Count:26
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Tensile Strength, Yield 44.0 - 120 MPa
6380 - 17400 psi
Average value: 55.2 MPa Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..