Polymer Property : Tensile Strength, Yield = 47.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 - 47.6 MPa
4000 - 6900 psi
Average value: 35.2 MPa Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Tensile Strength, Yield 47.2 - 47.6 MPa
6850 - 6900 psi
ASTM D638M
DSM Somos® GP Plus 14122
Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually ..