Polymer Property : Tensile Strength, Yield = 4786 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.00 MPa
4786 psi
At 50 mm/min; ISO 527-2
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according..