Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4830 MPa | 701000 psi | Typical fiber property |
Hexcel® HexTow™ AS7 Carbon Fiber HexTow™ AS7 carbon fiber is a continuous, high strength, high strain, PAN based fiber available, in a 12,000 (12K) filament count tow. This fiber has been surface treated and can be sized to improv.. |