Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 400 - 485 MPa | 58000 - 70300 psi | |
ArcelorMittal FB 540 Hot rolled ferrite-bainite steel Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: FB 450, 540, 560 and 590. This family of steel.. |