Tensile Strength, Yield 5.0925 MPa
738.61 psi
-3% change after 72 hours @ 200°C; ASTM D412
Precision Polymer Engineering S60S Silicone Rubber
Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Excellent steam resistance. Formulated using only those ingredients determi..