Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 50.3 MPa | 7300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 78761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Network Polymers Nylon 6615 L Description: Black Super Tough NylonInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)& Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Albis Plastics Polypropylene A 12 H-GK20/GF20 C , 20% Glass Bead/20% Glass Fiber
(discontinued **) Semi-crystalline Polypropylene Homopolymer (PPHP)Characteristics: Chemically Coupled Fiber; Good Dimensional StabilityApplications: Appliances, Furniture, Cases, Packaging and NoveltiesProcessing: I.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 IM HS L BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 IM L W Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 IM L W N Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 IM X Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF4 IM L LE Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Electrablend® ABS 03009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Information provided.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Electrablend® ABS SS5 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Statiblend® ABS LE Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Low Extractables and Semi ConductiveInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Electrablend® ABS SS7 BK MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES Electrablend® PA6 IM B Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Conductive, Impact Modified, Heat Stabilized and LubricatedAppearance: Off-WhiteInformation.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 FR-N IM Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Flame Retardant, Heat Stabilized, Impact Modified, Halogen Free and Lubricated Appearance: .. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM 638 |
PlastxWorld CEVIAN® S3100 PC/ABS alloy Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ASA S-150E-1115 ASA Weatherable Polymers Extrusion Grade, Medium Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Ensinger PVC Polyvinylchloride (PVC) Ensinger's type 1 grey PVC ROD is designed for machining solutions and is a cost effective solution for general industrial applications. The material offers an excellent combination of chemical resi.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D-638 |
Axiall HR-5009 Rigid PVC, Molding Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which incl.. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D-638 |
Axiall NR-5009 Rigid PVC, Molding Georgia Gulf NR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent processability, .. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D-638 |
Axiall 9175 White 10 Rigid PVC, Molding, White 10 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-10FG-0570 10% Glass Fiber Reinforced, Flame Retardant Information provided by Asahi Thermofil |