Network Polymers Nylon 6615 L

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Nylon 6615 L.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Black Super Tough NylonInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hours Immersion; ASTM D570
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 50.3 MPa
7300 psi
ASTM D638
Elongation at Break 50 - 60 %
50 - 60 %
ASTM D638
Flexural Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Notched 8.01 - 9.08 J/cm
15.0 - 17.0 ft-lb/in
1/8 in specimen; ASTM D256
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 1.33 - 1.60 J/cm
2.50 - 3.00 ft-lb/in
ASTM D256
1.33 - 1.60 J/cm

@Temperature -40.0 °C
2.50 - 3.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D648