Polymer Property : Tensile Strength, Yield = 508 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.50 MPa
508 psi
At 100% elongation, across flow; ASTM D412
Advanced Elastomer Systems VistaFlex® 714-B Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Tensile Strength, Yield 3.50 MPa
508 psi
At 100% elongation, across flow; ASTM D412
Advanced Elastomer Systems VistaFlex® 714-N Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Tensile Strength, Yield 3.50 MPa
508 psi
ASTM D638
Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer
Specially developed for high specification coating where metal/coating adhesion is of primary importance. Typically used on large flat surfaces, and when toughness, elasticity and excellent barrier ..
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate
Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly..
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate
Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane et..
Tensile Strength, Yield 3.50 MPa
508 psi
ASTM D638
Micropol E188 Rotational molding powder based on a random EVA copolymer
Information provided by Micropol Limited
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength, Yield 3.50 MPa
508 psi
at 100% elongation, maximum
Dow Corning SILASTIC® 25787 SILICONE RUBBER NATURAL
Information provided by Dow Corning
Tensile Strength, Yield 3.50 MPa

@Temperature 23.0 °C
508 psi

@Temperature 73.4 °F
ASTM D638
DuPont™ Surlyn® 9320 Zinc Ionomer
Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin ..
Tensile Strength, Yield 3.50 MPa

@Strain 100 %
508 psi

@Strain 100 %
Daikin DAI-EL LT-302 Fluoroelastomer, Low Temperature Grade, 64% Fluorine Content
Features: Flexible up to -30°C, excellent low temperature sealing.Information provided by Daikin Industries.
Tensile Strength, Yield 3.50 MPa
508 psi
chs 20 in/min; 100% elongation; ASTM D412
Diamond Polymers Softflex® 1302 Thermoplastic Elastomer Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 3.50 MPa
508 psi
ASTM D638
Arkema Group OREVAC® 9318 EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..
Tensile Strength, Yield 3.50 MPa
508 psi
50 mm/min
Arkema Group Evatane® 1020 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding flexible articles. Examples: fittings, rail pads, medical.ISO data provided by the manufacturer, Arkema.
Tensile Strength, Yield 3.50 MPa
508 psi
50 mm/min
Arkema Group Evatane® 1020 VG 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high mechanical properties. Examples: films, chemical bags, gloves.ISO data provided by the manufactur..
Tensile Strength, Yield 3.50 MPa
508 psi
ISO 527
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
Tensile Strength, Yield 3.50 - 38.0 MPa
508 - 5510 psi
Average value: 22.1 MPa Grade Count:57
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..