Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.52 MPa | 510 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4565 VAROX Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.52 MPa | 510 psi | at 100%; ASTM D412 |
2074A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 3.52 MPa | 510 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.52 MPa | 510 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3630 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |