Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synprene® RT-3630 Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3630 Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 32
32
Instant; ASTM D2240
Tensile Strength, Yield 3.52 MPa
510 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
2.21 MPa

@Strain 300 %
320 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 425 %
425 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 10.5 kN/m
60.0 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 15 %
15 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Users viewing this material also viewed the following: