Mechanical Properties Metric English Comments
Tensile Strength, Yield 538 MPa

@Strain 0.200 %,
Temperature 871 °C
78000 psi

@Strain 0.200 %,
Temperature 1600 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Tensile Strength, Yield 538 MPa
78000 psi
Universal Wire Works 90SB-3 Steel Welding Wire
Universal 90SB-3 is a 2.25% chromium and 1% molybdenum alloy for welding on steel of similar composition. This alloy is designed for joints in process piping systems, boilers, or pressure vessels. W..
Tensile Strength, Yield 538 MPa
78000 psi
Universal Wire Works 90SB-3L Steel Welding Wire
The 90SB-3L alloy is the same as the 90SB-3 alloy with the exception of a restricted carbon content. Universal 90SB-3 is a 2.25% chromium and 1% molybdenum alloy for welding on steel of similar comp..
Tensile Strength, Yield >= 538 MPa
>= 78000 psi
Eagle Brass 18665 MSP1, Spring
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Tensile Strength, Yield 538 - 655 MPa
78000 - 95000 psi
0.2% offset
Eagle Brass 521 Phosphor Bronzes 8% C, Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Yield 538 - 689 MPa
78000 - 100000 psi
0.2% offset
Eagle Brass 64725 MAX251C, Hard
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In..
Tensile Strength, Yield 538 - 607 MPa
78000 - 88000 psi
0.2% offset
Eagle Brass 715 Copper Nickel 30%, Extra Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Strength, Yield 538 - 641 MPa
78000 - 93000 psi
0.2% offset
Eagle Brass 725 Copper Nickel Tin, Extra Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Strength, Yield >= 538 MPa
>= 78000 psi
0.2% offset
Eagle Brass 735 Nickel Silver 18%, Extra Spring
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Tensile Strength, Yield 538 MPa

@Strain 0.200 %,
Temperature 566 °C
78000 psi

@Strain 0.200 %,
Temperature 1050 °F
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Yield 538 MPa
78000 psi
Universal Wire Works 122 Nickel Alloy Welding Wire
Alloy 122 is used for welding of nickel-chromium-molybdenum alloys as well as for overlay cladding on carbon, low alloy, or stainless steels. Alloy 122 is often used on dissimilar joints between nic..