Material Notes:
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.77 g/cc
0.317 lb/in³
Annealed
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 600 - 696 MPa
87000 - 101000 psi
Tensile Strength, Yield 538 - 689 MPa
78000 - 100000 psi
0.2% offset
Elongation at Break >= 5.0 %
>= 5.0 %
in 2 in.
Tensile Modulus 131 GPa
19000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.1 µm/m-°C

@Temperature 20.0 - 300 °C
9.50 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 15.91 W/m-K
110.4 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 96 %
96 %
Nickel, Ni 2.0 %
2.0 %
Silicon, Si 0.50 %
0.50 %
Tin, Sn 0.50 %
0.50 %
Zinc, Zn 1.0 %
1.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000481 ohm-cm
0.00000481 ohm-cm
Annealed