Tensile Strength, Yield 386 MPa
56000 psi
Materion BrushBronze® 95510 (AMS 4880) Continuous Cast 4.0" - 17.0"
Information supplied by Brush Wellman Engineered Materials.BrushBronzeâ„¢ 95510 is an Aluminum-Nickel-Bronze alloy that combines high strength, ductility, and good abrasion resistance under sever..
Tensile Strength, Yield 386 MPa

@Diameter 12.7 mm
56000 psi

@Diameter 0.500 in
Kaiser 6033 T8 Rod & Bar
Alloy 6033 is a higher strength version of alloy 6061, approaching properties typically obtainable with 2000 series alloys. The alloy was developed to also offer improved machinability over 6061. Th..
Tensile Strength, Yield 386 MPa

@Strain 0.200 %
56000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield >= 386 MPa
>= 56000 psi
Alcoa Excalibar® 6013-T8 Aluminum, 1.9-3.8 cm diameter
Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance...
Tensile Strength, Yield 386 MPa
56000 psi
EDRO #45 Free Machining Carbon Steel
EDRO #45™ is a medium carbon steel stocked in as rolled condition. EDRO #45™ is characterized by: excellent machinability, responds to surface hardening, may be welded, and good dimensional stabil..
Tensile Strength, Yield 386 MPa

@Diameter <=15.9 mm
56000 psi

@Diameter <=0.625 in
Rod
CMW® 28 Copper Alloy
CMW® 28 material is a copper base alloy having very high electrical and thermal conductivity and medium strength and toughness. It is a heat treatable alloy and develops its strength and hardness t..
Tensile Strength, Yield 386 MPa

@Strain 0.200 %
56000 psi

@Strain 0.200 %
AK Steel 18 SR® Ferritic Stainless steel
AK Steel 18 SR® provides excellent resistance to high temperature scaling - far superior to that of Type 446 stainless steel. This material is readily welded by conventional methods. It is not su..
Tensile Strength, Yield 386 MPa

@Temperature 260 °C
56000 psi

@Temperature 500 °F
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel
Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s..
Tensile Strength, Yield 386 MPa

@Temperature 204 °C
56000 psi

@Temperature 399 °F
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel
Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s..
Tensile Strength, Yield 386 MPa

@Strain 0.200 %,
Temperature 400 °C
56000 psi

@Strain 0.200 %,
Temperature 752 °F
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Tensile Strength, Yield 386 MPa

@Strain 0.200 %
56000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..