Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.07 MPa
590 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7344 Highly Saturated Nitrile Rubber
HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 4.07 MPa
590 psi
100%; ASTM D412
Teknor Apex APEX® 3310-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Tensile Strength, Yield 4.07 MPa
590 psi
at 150% Elongation, maximum
Dow Corning SILASTIC® LSR 9791-70 A&B KIT
70 Durometer, 2-part, 1 to 1 mix, translucent, molding grade, Liquid Silicone Rubber.Information provided by Dow Corning
Tensile Strength, Yield 4.07 MPa
590 psi
100%; ASTM D412
Teknor Apex APEX® 2565-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Tensile Strength, Yield 4.07 MPa
590 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-180 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 4.07 MPa
590 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-5155 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo..