Dow Corning SILASTIC® LSR 9791-70 A&B KIT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® LSR 9791-70 A&B KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
70 Durometer, 2-part, 1 to 1 mix, translucent, molding grade, Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc

@Temperature 25.0 °C
1.16 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Tensile Strength, Ultimate 10.0 MPa
1450 psi
Tensile Strength, Yield 4.07 MPa
590 psi
at 150% Elongation, maximum
Elongation at Break 450 %
450 %
Tear Strength 103 kN/m
590 pli
Compression Set 57 %
57 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
3.0

@Frequency 100000 Hz
3.0

@Frequency 100000 Hz
Dielectric Strength 17.7 kV/mm
450 kV/in
Dissipation Factor 0.0019

@Frequency 100 Hz
0.0019

@Frequency 100 Hz
0.015

@Frequency 100000 Hz
0.015

@Frequency 100000 Hz
Processing Properties Metric English Comments
Pot Life 1440 min
1440 min
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance translucent
Mix Ratio (X:1) 100
Base to Catalyst ETN