Mechanical Properties Metric English Comments
Tensile Strength, Yield 413 - 517 MPa
59900 - 75000 psi
With 0% cold work
OMG Americas GlidCop® AL-60 Dispersion Strengthened Copper
GlidCop® AL-60 is copper that is dispersion strengthened with 1.1 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o..
Tensile Strength, Yield 448 - 517 MPa

@Strain 0.200 %
65000 - 75000 psi

@Strain 0.200 %
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 448 - 517 MPa

@Strain 0.200 %
65000 - 75000 psi

@Strain 0.200 %
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 483 - 517 MPa

@Strain 0.200 %
70000 - 75000 psi

@Strain 0.200 %
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 483 - 517 MPa

@Strain 0.200 %
70000 - 75000 psi

@Strain 0.200 %
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 414 - 517 MPa
60000 - 75000 psi
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron
Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r..
Tensile Strength, Yield 483 - 517 MPa

@Strain 0.200 %
70000 - 75000 psi

@Strain 0.200 %
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 421 - 517 MPa
61000 - 75000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield 352 - 517 MPa
51000 - 75000 psi
0.2% offset
Eagle Brass 521 Phosphor Bronzes 8% C, 1/2 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Yield 345 - 517 MPa
50000 - 75000 psi
Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze
Finished product available as bar,rod, forged, shapes, or tubes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chica..
Tensile Strength, Yield 483 - 517 MPa
70000 - 75000 psi
Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy
Finished product available as bar, wire, or rod.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Meta..
Tensile Strength, Yield 345 - 517 MPa

@Strain 0.200 %
50000 - 75000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899A 1/2 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 345 - 517 MPa

@Strain 0.200 %
50000 - 75000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899L 1/2 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 345 - 517 MPa

@Strain 0.200 %
50000 - 75000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899M 1/2 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 345 - 517 MPa

@Strain 0.200 %,
Thickness <=25.4 mm
50000 - 75000 psi

@Strain 0.200 %,
Thickness <=1.00 in
Cold Drawn Bars
Schmolz + Bickenbach IMRE™ Stainless Steel Bar
Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand..